Fabrication of n-type Bi₂Te₃ film using electrophoretic deposition for thermoelectric applications

Files

hdl_114567.pdf (1.5 MB)
  (Accepted version)

Date

2018

Authors

Talebi, T.
Ghomashchi, R.
Talemi, P.
Aminorroaya, S.

Editors

Advisors

Journal Title

Journal ISSN

Volume Title

Type:

Journal article

Citation

Surface and Coatings Technology, 2018; 343:127-130

Statement of Responsibility

Tahereh Talebi, Reza Ghomashchi, PejmanTalemi, Sima Aminorroaya

Conference Name

Abstract

Fabrication of uniform, crack-free n-type Bi2Te3 films using a fast, cost-effective, electrophoretic deposition method for thermoelectric applications has been reported in this study. The sintering process has been done at 693 K to achieve compact and dense coatings. The microstructures of the surface of the green and sintered films, as well as their thicknesses, have been investigated using SEM, which showed a uniform and even film has resulted using electrophoretic deposition (EPD). Furthermore, the Seebeck coefficients of the green and sintered films have been measured and in-plane Seebeck coefficients of 189 μV/K have been recorded for the sintered film at 500 K.

School/Discipline

Dissertation Note

Provenance

Description

Access Status

Rights

© 2017 Elsevier B.V. All rights reserved.

License

Grant ID

Call number

Persistent link to this record