Enhancing toughness of CrN coatings by Ni addition for safety-critical applications

dc.contributor.authorWo, P.
dc.contributor.authorMunroe, P.
dc.contributor.authorJiang, Z.
dc.contributor.authorZhou, Z.
dc.contributor.authorLi, K.
dc.contributor.authorXie, Z.
dc.date.issued2014
dc.description.abstractAbstract not available
dc.description.statementofresponsibilityPui Ching Wo, Paul R. Munroe, Zhong-Tao Jiang, Zhifeng Zhou, Kwok Yan Li, Zonghan Xie
dc.identifier.citationMaterials Science and Engineering A: Structural Materials: Properties, Microstructure and Processing, 2014; 596:264-274
dc.identifier.doi10.1016/j.msea.2013.12.064
dc.identifier.issn0921-5093
dc.identifier.issn1873-4936
dc.identifier.urihttp://hdl.handle.net/2440/89698
dc.language.isoen
dc.publisherElsevier Science SA
dc.rights© 2013 Elsevier B.V. All rights reserved.
dc.source.urihttps://doi.org/10.1016/j.msea.2013.12.064
dc.subjectCrNiN; Cross-sectional transmission electron microscopy; Damage tolerance; Nanoindentation; X-ray photoelectron spectroscopy
dc.titleEnhancing toughness of CrN coatings by Ni addition for safety-critical applications
dc.typeJournal article
pubs.publication-statusPublished