Mechanism for zincophilic sites on zinc-metal anode hosts in aqueous batteries

dc.contributor.authorXie, F.
dc.contributor.authorLi, H.
dc.contributor.authorWang, X.
dc.contributor.authorZhi, X.
dc.contributor.authorChao, D.
dc.contributor.authorDavey, K.
dc.contributor.authorQiao, S.Z.
dc.date.issued2021
dc.description.abstractThe zinc‐metal anode (ZMA) is a critical component of rechargeable Zn‐based batteries. Zinc‐dendrite formation on ZMA during cycling causes an internal short‐circuit, thereby limiting long‐term practical operation of batteries. A strategy of introducing zincophilic sites shows promise in suppressing dendrite growth. However, the mechanism is not understood. Here, a detailed study of the mechanism of zincophilic sites based on multiple in situ/ex situ techniques is reported. Using a carbon‐host as a model system with nitrogen sites as zincophilic sites and both ex situ near‐edge X‐ray absorption fine structure (NEXAFS) and in situ Raman spectra, it is shown that zinc ions are bonded with pyridine sites to form Zn–N bonds. The Zn–N bonds induce spacious nucleation of zinc on carbon‐hosts and suppress zinc‐dendrite formation. The host with zincophilic sites exhibits a homogenous Zn deposition, together with boosted electrochemical performance. This finding underscores the impact of nitrogen zincophilic sites in suppressing zinc‐dendrite formation. It is shown that bonding between zinc ions and zincophilic sites is the mechanism for zincophilic nucleation in the ZMA host. These findings are expected to be of immediate benefit to researchers in battery technologies and materials science.
dc.description.statementofresponsibilityFangxi Xie, Huan Li, Xuesi Wang, Xing Zhi, Dongliang Chao, Kenneth Davey, and Shi-Zhang Qiao
dc.identifier.citationAdvanced Energy Materials, 2021; 11(9):2003419-1-2003419-8
dc.identifier.doi10.1002/aenm.202003419
dc.identifier.issn1614-6832
dc.identifier.issn1614-6840
dc.identifier.orcidXie, F. [0000-0002-6133-6558]
dc.identifier.orcidLi, H. [0000-0003-0662-6939]
dc.identifier.orcidWang, X. [0000-0002-2477-8111]
dc.identifier.orcidZhi, X. [0000-0001-9387-3465]
dc.identifier.orcidChao, D. [0000-0001-7793-0044]
dc.identifier.orcidDavey, K. [0000-0002-7623-9320]
dc.identifier.orcidQiao, S.Z. [0000-0002-1220-1761] [0000-0002-4568-8422]
dc.identifier.urihttp://hdl.handle.net/2440/129952
dc.language.isoen
dc.publisherWiley
dc.relation.granthttp://purl.org/au-research/grants/arc/DP160104866
dc.relation.granthttp://purl.org/au-research/grants/arc/DE20010124
dc.relation.granthttp://purl.org/au-research/grants/arc/FL170100154
dc.rights© 2021 Wiley-VCH GmbH
dc.source.urihttps://doi.org/10.1002/aenm.202003419
dc.subjectAqueous batteries; deposition; nucleation; zinc-metal anodes; zincophilic sites
dc.titleMechanism for zincophilic sites on zinc-metal anode hosts in aqueous batteries
dc.typeJournal article
pubs.publication-statusPublished